Barb & Dan Artley wrote:
> The stainless bar end housing is only good if you're making it period
> correct, but even then most folks I knew replaced it with vinyl coated
> and as soon as it was available, nylon or Teflon? lined housing. The
> spiral stainless is a total loss grease system. You'll lose all the
> grease on the first hot day.
One brand of teflon-lined housing available in the early 80s had a liner that could be readily removed from the housing. I pulled enough of this teflon liner out to use with the stainless housing (it slid right in, problem) and have been using it that way ever since.
--
-John Thompson (john@os2.dhs.org)
Appleton WI USA