Re: [CR]Mavic MA40 vs Mavic MA2 question on Anodizing

(Example: Framebuilding:Technology)

From: "David Joshel" <davidjoshel@hotmail.com>
To: "Mark Cutrufelli" <rena.cutrufelli@comcast.net>, <classicrendezvous@bikelist.org>
References: <MONKEYFOOD7qIA3EEmY000007ff@monkeyfood.nt.phred.org> <558150.37559.qm@web51501.mail.re2.yahoo.com> <000f01c8a5ad$682d3ea0$0d0a0a0a@PC175064711631>
Subject: Re: [CR]Mavic MA40 vs Mavic MA2 question on Anodizing
Date: Wed, 23 Apr 2008 20:29:14 -0700
reply-type=original

Hi Mark, All

The MA2's are clear or silver anodized, but to not hard anodized like the MA40's. IMO the MA2's are the choice over the MA40. I believe they used the same extrusion mold to produce both, but because of the hard anodizing on the MA40's, those are more likely to crack. I have several pairs of really old MA2 wheelsets that have not cracked at the spokeheads, and the one set of MA40's I had did crack at the spokeheads.

DAve Joshel
Davis CA USA


----- Original Message -----
From: Mark Cutrufelli
To: classicrendezvous@bikelist.org
Sent: Wednesday, April 23, 2008 6:49 PM
Subject: [CR]Mavic MA40 vs Mavic MA2 question on Anodizing



>
>
> I currently have a pair of both. I know the 40's are hard anodized-they
> are
> dk grey, nearly black. While the MA2s are silver , I know they are not
> hard
> anodized but are they anodized at all? I ask because if the MA2's are
> totally unanondized, then I can polish to my heart's content.
>
>
>
> Mark Cutrufelli
> Laurel, Maryland
> USA